http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09276780-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dc45703f67bc72a6db582867886fd5d5 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-36 |
filingDate | 1996-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bc361ef9f352728c60b7e8803cd98831 |
publicationDate | 1997-10-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09276780-A |
titleOfInvention | Method for forming waterproof coating |
abstract | (57) Abstract: [PROBLEMS] To improve the water resistance of a coating film by enabling sufficient reaction and removal of at least OH groups present on the surface portion of the coating film. SOLUTION: A coating film forming step of forming a coating film by applying a coating material to a coating object, and a reactive functional group for changing an OH group in the coating film into a functional group having a higher hydrophobicity than the OH group. And a reaction composition for reacting the reactive composition having the above-mentioned with the above coating film to change the OH group present at least on the surface of the coating film into a functional group having a higher hydrophobicity than the OH group. Characterize. By changing the OH group existing on the surface of the coating film to a hydrophobic functional group, the water resistance of the coating film can be reliably improved. |
priorityDate | 1996-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |