http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09263679-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 |
filingDate | 1996-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79115fbb026135a5ad34a03e62629280 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de1310cf335082ffd9c042051477481b |
publicationDate | 1997-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09263679-A |
titleOfInvention | Soft propylene-α-olefin block copolymer composition |
abstract | (57) Abstract: [PROBLEMS] To provide a soft propylene-α-olefin block copolymer composition which can be fused by high frequency or microwave and has good adhesiveness. SOLUTION: (A) Polypropylene block (a) And propylene and 2 to 12 carbon atoms (excluding 3) Of α-olefin copolymer elastomer block (b), and the elastomer block (b) accounts for 20 to 70% by weight of the total copolymer, and the polypropylene block (a) matrix phase has an elastomer block. Soft propylene-α-olefin block copolymer 100 in which (b) exists in a dispersed state, and the dispersed particles have a number average particle diameter of 1.0 μm or less and an area average particle diameter of 1.5 μm or less. Parts by weight and (B) a compound having a hydroxyl group in the molecular chain 0.5 to 30 parts by weight, Or (C) 0.01 to 20 parts by weight of an aluminosilicate of an alkali metal or an alkaline earth metal. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005133024-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006212785-A |
priorityDate | 1996-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 117.