http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09250026-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 |
filingDate | 1996-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4d3150bfbd1a35a8d150f8ba0a3f235 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_71bf0d69881a910b70b431364dea083f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e5aa07ceab76085e6f6247775d5bd771 |
publicationDate | 1997-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09250026-A |
titleOfInvention | Black-dyed polyester fiber |
abstract | (57) 【Abstract】 PROBLEM TO BE SOLVED: The flatness of the fiber surface is excellent, the wear of the rollers, guides, etc. that come into contact during spinning or molding of the obtained fiber is small, and the wear of accessories during use and the fiber To provide a black-dyed polyester fiber with little strength deterioration. SOLUTION: The average primary particle size is 5 to 25 mμ, the oil absorption is 30 to 80 ml / 100 g, and the specific surface area is 150 to 3. Carbon black having a characteristic of 00 m 2 / g is blended in the polyester fiber in an amount of 0.3 to 1.0% by weight. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003089971-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022080086-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010032113-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4674429-B2 |
priorityDate | 1996-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 24.