http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09249675-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7ad58d3c0b071069a8ee0cb8c8ba2e8 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B17-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07F7-1892 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-548 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B17-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B17-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F7-18 |
filingDate | 1997-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75277955b491cf15c346b973fc9f5d7f |
publicationDate | 1997-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09249675-A |
titleOfInvention | Method for producing polysulfide silyl ethers |
abstract | (57) Abstract: A method for producing polysulfide silyl ethers. Starting from hydrated metal sulphides and / or metal polysulphides, which are optionally in vacuum or under pressure at temperatures of 90 to 220 ° C., in the presence of water-immiscible organic solvents and It is first dehydrated in the presence of an emulsifier and, if metal sulfides are used, then they are reacted with sulfur to give metal polysulfides, and then the resulting dehydrated metal polysulfides are To 150 ° C The reaction of the metal polysulfide with the halogenoalkylsilanes is carried out in the presence of a polyhalogenated compound at any temperature so as to change the corresponding polysulfide silylethers with halogenoalkylsilanes. Manufactures. |
priorityDate | 1996-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 185.