Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f2e1eed951518d6a42752736e3fd3afb |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25F1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23G1-12 |
filingDate |
1996-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34a0d8a2e89385a69d34f216e5f96148 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43124c5d449267921aa62f0a7817e31e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eed2b5bdc2b6bd86827ec1773f17e703 |
publicationDate |
1997-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H09241897-A |
titleOfInvention |
Pretreatment method for magnesium or its alloy surface |
abstract |
(57) 【Abstract】 PROBLEM TO BE SOLVED: To eliminate the need for exhausting or cleaning equipment, to excel in the cleaning ability as a pretreatment, and to improve the adhesion and corrosion resistance of the subsequent surface treatment. Provide a pretreatment method. A method for pretreatment of magnesium or its alloy, which comprises cleaning the surface of magnesium or its alloy by pickling and further performing anodic electrolytic treatment. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H11293500-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014203919-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2014203919-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006299328-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104404612-A |
priorityDate |
1996-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |