http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09216957-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2f8cfa5aee4410611b5c562275c9f8e3 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K25-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 |
filingDate | 1996-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a65bc88306ae7a08b347de131897c1ef |
publicationDate | 1997-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09216957-A |
titleOfInvention | Biaxially stretched polystyrene resin sheet |
abstract | (57) [Abstract] [PROBLEMS] To provide a biaxially stretched polystyrene-based resin sheet which is excellent in oil resistance, weakens the blocking of stretched sheets from each other, and has good container deep drawing property and good peeling property due to stacking of molded products. SOLUTION: The polystyrene-based resin has an average particle size of 1 to 5 μm. 1 to 10% by weight of styrene-grafted diene rubber having a rubber swelling degree of 9 to 15 and a rubber concentration of 1 to 10% by weight, and an organic crosslinked fine particle having an average particle diameter of 0.5 to 10 μm. A biaxially stretched polystyrene-based resin sheet, which is obtained by biaxially stretching a resin composition containing 0.00 to 1000 ppm. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-1321151-C |
priorityDate | 1996-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 37.