Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_00247449e91da784127a524fa801e8fb |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F11-14 |
filingDate |
1996-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_07dba3a3fc02d981a7b1688fd6f791aa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_49004b52bcb390761ec8b4b60470815d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_367dbbf7e17fc2481564d1bb04fe0dea http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_127dc8dad5075437c56b7860ee1cb787 |
publicationDate |
1997-07-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H09192699-A |
titleOfInvention |
Sludge treatment method and sludge treated material for cement raw material |
abstract |
(57) 【Abstract】 PROBLEM TO BE SOLVED: To significantly reduce running cost and to effectively reduce sludge by significantly reducing the amount of quicklime used with a very small amount of energy and cost. The present invention provides a sludge treatment method and a sludge treated product for cement raw material, which can be stably and effectively utilized. SOLUTION: The sludge having a water content of 60% or more is mixed with quicklime, and the water content of the mixture is set to 15% or more and less than 60%, preferably 20% or more and less than 35%. . |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113801992-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20220085443-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113801992-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011013491-A1 |
priorityDate |
1996-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |