http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09183838-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_997ed5b3b186e8e8ddd4b0f8685a1d12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-00 |
filingDate | 1995-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_018a5b03942234a225c3498cad83c6dc |
publicationDate | 1997-07-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09183838-A |
titleOfInvention | Method for producing aromatic polycarbonate resin |
abstract | (57) 【Abstract】 PROBLEM TO BE SOLVED: To maintain moldability, while maintaining excellent transparency and mechanical properties of an aromatic polycarbonate resin suitable for optical materials. Provided is a method for producing an aromatic polycarbonate resin, which has good thermal stability and mold corrosion resistance and gives a molded article having low birefringence. At least 80 mol% of the wholly aromatic dihydroxy component comprises (a) 1,1-bis (4-hydroxyphenyl) -3,3,5-trimethylcyclohexane and (b) 2,2-bis (3-). A method for producing an aromatic polycarbonate resin, which comprises melt-polymerizing an aromatic dihydroxy component having a specific ratio of methyl-4-hydroxyphenyl) propane and a carbonic acid diester. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002533508-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012520906-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010105769-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102009013643-A1 |
priorityDate | 1995-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 517.