abstract |
(57) Abstract: [PROBLEMS] To provide an antistatic polyester film having excellent coating appearance and antistatic properties under low humidity, and excellent abrasion resistance. The polyester film has at least one surface. (1) Ratio of phosphate ester antistatic agent 5 to 40% by weight, (2) Ratio of surfactant having HLB of 12 or less 1 to 20% by weight, (3) Acrylic copolymer and polyester copolymer Proportion of at least one binder component selected from coalescence 40 to 90% by weight and (4) Fluorine-based organic fine filler 0.1 An antistatic polyester film having improved abrasion resistance, which is obtained by applying a coating material containing a composition of from about 4% by weight and then drying and stretching to apply a coating film. |