http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09174665-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_01c1e0bc0628f76dea731cda5a666ca1 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-36 |
filingDate | 1995-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e42975746f7e1f8a2c10043b4b1f8c6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f84bd5957f3c603470033c018a7ca501 |
publicationDate | 1997-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09174665-A |
titleOfInvention | Method for producing foamed polyester resin sheet having excellent moldability |
abstract | (57) [Abstract] [PROBLEMS] To produce a polyester resin foam sheet having excellent moldability. SOLUTION: An extruded foamed sheet having a thickness of 0.5 to 3.0 mm using a polyester-based resin as a base resin is heated to a temperature not lower than the glass transition temperature and not higher than a temperature 20 ° C. lower than the crystallization temperature. The crystallinity of one surface portion and the crystallinity of the other portion are each 15% or less, In addition, the difference between the crystallinity of one surface portion of the sheet and the crystallinity of the other surface portion is set to 2% or less. |