abstract |
(57) [Summary] (Corrected) [PROBLEMS] To provide a polyphenylene ether / polyamide resin composition having high Izod impact strength, high tensile elongation, and the like. SOLUTION: (A) Polyphenylene ether 5-9 0 wt% (B) B-1 Polyamide-1, B-2 Polyamide- 2 95 to 10% by weight in total (C) C-1 rubber-1, C-2 rubber-2, C-3 Rubber-3 (D) Polyamide and polyphenylene ether compatibilizer 0.01 to 30 parts by weight are prepared, and (i) Extruder No. 1 The components (D), (A) and (C-1) are fed from the supply port of (1) and melt-kneaded, and (ii) from the second supply port (B). -1) and (C-2) components are fed, melt-kneaded with (i), and (iii) the (B-2) and (C-3) components are fed from the third supply port, ii) and a method of producing a thermoplastic resin composition, which comprises melt-kneading. |