http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09143879-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ebe9a0fef022f57edb726997a3f666ac |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M101-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-333 |
filingDate | 1995-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e7e289b435e0e8286cb6c40872db9cb3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9a1e16644c0cfe4041eabd475dab732c |
publicationDate | 1997-06-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09143879-A |
titleOfInvention | Sizing agent for fiber sizing |
abstract | (57) [Summary] [Purpose] A cost-effective paste for fiber sizing that retains the excellent suitability of polyvinyl alcohol-based paste for fiber sizing and improves the divide property, which is a drawback of polyvinyl alcohol-based paste. provide. [Structure] Polyvinyl alcohol (A) and polyvinyl alcohol polymer (B) having an alkyl group having 2 or more carbon atoms, and the weight ratio of polyvinyl alcohol (A) / polyvinyl alcohol polymer (B) is 99. 5 / The main component is a composition of 0.5 to 0.5 / 99.5. |