http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09128824-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d9cb217f83556ce2a418344c2d485415 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B11-105 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B11-10 |
filingDate | 1995-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c991e958c6588a022afa47874582f9e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_89d3751e0440ba42622917f2704c86ee http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_887eefa55da46139f9d6895b353ac2ef |
publicationDate | 1997-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09128824-A |
titleOfInvention | Magneto-optical recording medium |
abstract | (57) [Abstract] [Problem] It is possible to stably record and reproduce by light, Provided is a magneto-optical recording medium having excellent corrosion resistance, a large magneto-optical effect, and excellent productivity. A substrate is represented by the following general formula (I), A Curie temperature is in the range of 80 to 200 ° C., and a magnetic layer composed of a hexagonal ferrite magnetic powder having an average particle diameter of 3 to 300 nm and a binder is provided. AO · n (Fe 12-xy M1 x M2 y O 18-Z ) (I) (wherein A represents one or more elements selected from Ba, Sr, Ca and Pb, and M1 represents Co, Ni, One or more elements selected from Zn, Ti, Zr, Sn, Nb and Sb, M2 is Al, Cr And one or more elements selected from Ga and n = 0.8 ~ 2.0, x = 0.1 to 5.0, y = 2.5 to 6.0, z = (3-m) x / 2 (m represents the average valence of M1). ) |