http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H09102308-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_345d74727e77e6d36988fd1168fb2589 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 |
filingDate | 1995-10-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79db6b9f827e59ac456092e752319ae9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c4c9e70d7328f2aa5b82d2c1309780a6 |
publicationDate | 1997-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H09102308-A |
titleOfInvention | Alkaline secondary battery |
abstract | (57) Abstract: It is an object to provide an alkaline secondary battery having an improved charge / discharge cycle life by improving a negative electrode containing a hydrogen storage alloy. SOLUTION: A positive electrode 2 and a negative electrode 4 containing a hydrogen storage alloy And a separator 3 interposed between the positive electrode 2 and the negative electrode 4 and an alkaline electrolyte. In the alkaline secondary battery, the negative electrode 4 is added to a 6N potassium hydroxide aqueous solution at 45 ° C. The alkali absorption rate after immersion for 2 hours is 2 ˜20%. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20010073280-A |
priorityDate | 1995-10-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 32.