Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-42 |
filingDate |
1994-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4b446584f7abf75870d9fbe830f79fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a16246a7b17182e668436a613494613c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e53f4ea4f3dc9b98bcae457bb27389c |
publicationDate |
1996-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0881517-A |
titleOfInvention |
Method for producing boron-containing thermoplastic resin |
abstract |
(57) [Summary] [Structure] 0.0001 meq of double bond in extruder. / G or more of the thermoplastic resin (A) is reacted with a boron-hydrogen bond-containing boron compound (B), a method for producing a boron-containing thermoplastic resin. [Effect] According to the present invention, a boron-containing thermoplastic resin having good compatibility with a polymer having a multi-valued hydroxyl group such as an ethylene-vinyl alcohol copolymer can be easily synthesized by an extruder. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6949298-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006137873-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-02060961-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001310961-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006176788-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100830357-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4610690-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7109272-B2 |
priorityDate |
1994-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |