http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08504449-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F265-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F265-06 |
filingDate | 1993-11-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 1996-05-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08504449-A |
titleOfInvention | Plastic undercoating or single-layer coating method using water-based coating |
abstract | (57) Summary The present invention relates to a method for undercoating or single-layer coating of plastics using an aqueous coating agent containing, as a film-forming material, one or more emulsion polymers and a water-dilutable polyurethane resin. In this method, the aqueous coating agent comprises a), in the first step, 10 to 90 parts by weight of an ethylenically unsaturated monomer or a mixture of ethylenically unsaturated monomers, in an aqueous layer, one or more emulsifiers and a radical forming initiator. Polymerized in the presence of one or more agents, and b) after the reaction of at least 80% by weight of the ethylenically unsaturated monomer or monomer mixture used in the first step, in the second step, It contains an emulsion polymer obtained by polymerizing 90 to 10 parts by weight of a mixture of saturated or ethylenically unsaturated monomers in the presence of the polymer obtained in the first step, the reaction conditions being such that The emulsion polymer is selected to have a number average molecular weight of 200,000 to 2,000,000 and the emulsion polymer has a hydroxyl number of 2 to 100. And a glass transition temperature of the resulting polymer (T g1) in the first step (a), the second step (b) a mixture of the use of ethylenically unsaturated monomers with the use of the monomer or the second step (b) with In the ethylenically unsaturated monomer or monomer mixture used in the first step and in the second step, the absolute difference from the glass transition temperature (T g2 ) of the polymer that will be obtained by homopolymerization is 10 to 170 ° C. It is characterized in that the type and amount of ethylenically unsaturated monomer or mixture of monomers used is selected. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015505883-A |
priorityDate | 1992-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 188.