http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0839926-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 |
filingDate | 1995-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_295f9d360ded1e2c8da2613310e9161c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b4fa85e86008ec4e93adcbef08fff6d9 |
publicationDate | 1996-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0839926-A |
titleOfInvention | Recording material |
abstract | (57) Abstract: [PROBLEMS] To provide a full-color recording material for inkjet recording which satisfies various requirements for inkjet recording, particularly has high ink absorbability and excellent color developability. SOLUTION: Inorganic pigment particles 10 having a particle size of 3 to 20 μm A coating composition was prepared by mixing 20 to 100 parts by weight of a binder composed mainly of a water-soluble polymer with 0 part by weight, and a dry coating amount of 15 g / m 2 was prepared on a support. Coating is carried out as described above to form a coating layer on the surface of which the irregular particle shape of the inorganic filler particles appears, to obtain a recording material for inkjet recording. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100329975-B1 |
priorityDate | 1995-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 40.