http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H083714-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_242cc8d15c771395b920cc7de452da6a
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C4-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B3-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02
filingDate 1994-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc9bf0b53d89488118552fa7d193de54
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82c2cf65c16a9e87b79f4a673e96e245
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa76449ccaadd5d7d17b2749c864e018
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8ce09359bcb520a9e8c9b1b822e22efe
publicationDate 1996-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-H083714-A
titleOfInvention Method for manufacturing laminated body
abstract (57) [Summary] [Purpose] When forming a sprayed film on a dense sintered body such as an interconnector, by improving the adhesion between the dense sintered body and the sprayed film, they can be separated from each other. Prevent, Furthermore, it is to improve the airtightness between the two. [Structure] On a dense sintered body 1 having a relative density of 94% or more, a porous film 5 having open pores with a small opening and a widened inside is formed on the surface side, and then on the porous film 5. Then, the sprayed film 8 is formed by the spraying method. Preferably, A paste containing a raw material powder for a porous film, a dispersion medium, and a pore-forming agent is applied onto the dense sintered body 1 to form a coating layer, The porous film 5 is formed by baking this coating layer. Further, after forming the sprayed film 8, the sprayed film 8 is heat-treated to make the sprayed film 8 airtight.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0008701-A3
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002373675-A
priorityDate 1994-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451134653
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID165970
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID157428004
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID3014696
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID452576905
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID447950107

Total number of triples: 26.