assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_75249adb90a4cfa442d4751eea6ee07e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 |
filingDate | 1995-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9db56290b299c87854f252a61a66a6ef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1b61fee5ee35b8741ca4ff4073c718b5 |
publicationDate | 1996-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08332448-A |
titleOfInvention | Method of forming coating with design |
abstract | (57) [Summary] (Corrected) [Structure] Applying an undercoat paint on a metal plate, baking and curing, and then applying an intermediate paint containing a specific mixed resin and color pigment, and curing. No. 1 containing a specific mixed resin and color pigment at required locations on the intermediate coating without Applying a topcoat base paint, applying a first topcoat clear paint consisting of a specific mixed resin on the first topcoat basecoat without curing it, baking and curing it, and the required locations on the first topcoat clear film Is masked with a masking material, and the surface to be coated other than the masking contains a specific mixed resin and color pigment, but a second top coat paint of a color different from the first base coat paint is applied, and the entire painted surface is baked and cured. And removing the masking material to form a coating film having a design property. [Effect] It is possible to reduce the number of baking steps compared with the conventional one, and to have a design property, and it is also excellent in chipping resistance and peeling resistance due to stepping stones and the like. |
priorityDate | 1995-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |