http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08311419-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-10 |
filingDate | 1995-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f75e89567c4bd3e37b73045e31bdebf8 |
publicationDate | 1996-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08311419-A |
titleOfInvention | Surface protection film |
abstract | (57) [Abstract] [Purpose] To provide a surface protective film which has sufficient initial adhesiveness to an object to be protected, does not increase in adhesive strength after heat treatment, can be easily peeled off, and does not contaminate the object to be protected. . [Structure] On one surface of a base material layer made of a thermoplastic resin film, a temperature range from a temperature at which 10% by weight is eluted by a cross fractionation method to a temperature at which 100% by weight is completed is 30. C. or less, value of weight average molecular weight / number average molecular weight of 1.5 to 3.5, density of 0.840 to 0.920 g / c An adhesive layer made of m 3 polyethylene resin is formed. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008162108-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009148996-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013136791-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012082263-A |
priorityDate | 1995-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 38.