http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08302000-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-672 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-66 |
filingDate | 1995-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9b9dd577894f13f76d917d6c366cf59 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_33b64777a6b36e35a95ab714cc26b9b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f0ae30aa5e2c35e3f0ed9b8674887f9 |
publicationDate | 1996-11-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08302000-A |
titleOfInvention | Thermoplastic polyester elastomer |
abstract | (57) [Summary] [Object] To provide a thermoplastic polyester elastomer having a low content of THF and excellent in heat resistance and color tone. [Structure] A polyester elastomer containing aromatic dicarboxylic acid, 1,4-butanediol, and polytetramethylene glycol (PTMG) having a molecular weight of 400 to 6000 as main components, and the phosphoric acid content in PTMG is 5 to 20 p. A polyester elastomer having a pm and a fluorine content of 100 ppm or less and a tetrahydrofuran (THF) content (A) in the polymer satisfying the following formula (1). A / 20 <C / B (1) A: THF content (ppm) in elastomer, B: P Phosphoric acid content in TMG (ppm), C: Content of PTMG in elastomer (% by weight) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EA-009917-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005116111-A1 |
priorityDate | 1995-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.