http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08295542-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K55-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C71-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C27-12 |
filingDate | 1995-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3283e80f267944e980991959fac76fe8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_86dcf68e641e2bec55a830af26aa58e0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc0e2add1b490deebf76e8ec02e796eb |
publicationDate | 1996-11-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08295542-A |
titleOfInvention | Intermediate film and laminated glass |
abstract | (57) [Summary] [Structure] An interlayer film comprising an ethylene-vinyl acetate copolymer or an ethylene- (meth) acrylic acid ester copolymer and a transparency improving agent, and a laminated glass using the interlayer film. Therefore, the intermediate film 7 is subjected to plasma discharge treatment, and this plasma discharge treatment is performed between the pair of metal electrodes 4 and 5 on which the solid dielectric 6 is disposed on at least one of the facing surfaces. It is performed under a pressure near atmospheric pressure in an atmosphere of a mixed gas of a gas or a rare gas and an oxygen-containing gas or a nitrogen-containing gas. [Effects] Under conventional low pressure (eg 0.3 to 10 Torr) No expensive equipment such as a vacuum chamber or a vacuum exhaust device is required unlike the plasma discharge treatment in the above, and the manufacturing cost of the interlayer film and the laminated glass is reduced. Further, it is possible to obtain a laminated glass which has improved adhesiveness without using a silane coupling agent, has no yellowing, has good transparency, and has little change in adhesiveness with time. |
priorityDate | 1995-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 68.