http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08260242-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-84 |
filingDate | 1995-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bdf19f8d220e83fec5d72444a6b678c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d29214dc793ed9579cb7e73b6a0ee8a3 |
publicationDate | 1996-10-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08260242-A |
titleOfInvention | Liquid crystal polyester fiber |
abstract | (57) [Summary] (Modified) [Objective] To provide liquid crystal polyester fiber having high strength and elastic modulus and excellent in dyeability. A fiber comprising a melt-liquid crystal forming polyester, which has no shrinkage stress peak at 50 ° C to 250 ° C, and has a stress value (T1) of 200 at 50 ° C. The ratio of stress values (T2) at ° C satisfies the formula (1), and the dyeing parameter (Z) satisfies the formula (2), Further, a liquid crystal polyester fiber having a b value after dyeing blue of -5 or less. T1 / T2 ≦ 15 (1) Z = L1 / L2 ≧ 1.4 (2) (L1: L value of liquid crystal polyester fiber before dyeing, L2: L value of liquid crystal polyester fiber after blue dyeing) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011111696-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100305840-B1 |
priorityDate | 1995-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 36.