Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L79-08 |
filingDate |
1995-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e40235335a3365eff62cbc928d1765f0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f049358f2240179814bb0a894f5a11a7 |
publicationDate |
1996-10-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H08259746-A |
titleOfInvention |
Resin composition for microwave fusion |
abstract |
(57) [Abstract] [Purpose] Efficient heat generation by microwave irradiation, A resin composition for microwave fusion, which can be fused without deteriorating the resin and has high mechanical strength at the fused portion. [Structure] Unmodified polyolefin resin having a melt flow rate of 0.1 to 15 g / 10 min and a melt flow rate of 0.1 Conductive aniline polymer fine particles are mixed with an olefin resin composed of an ionomer resin or an unsaturated carboxylic acid (anhydride) -modified polyolefin resin in an amount of up to 20 g / 10 min. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015064652-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-0238669-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-1296421-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9922748-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6828362-B1 |
priorityDate |
1995-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |