abstract |
(57) [Summary] [Structure] Polyamide resin, partially saponified ethylene-vinyl acetate copolymer, higher fatty acid metal salt, 230 Melt index MFR (0) measured at 230 ° C. and 5000 g after heat treatment for 300 minutes at 220 ° C. and melt index MFR (0) measured at 5000 ° C. and 5000 g is Which is a resin composition. [Effect] The resin composition falling within the scope of the claims of the present invention is characterized in that it can easily form a homogeneous film for a long time, has excellent tie-pin hole properties at low temperatures, and can easily incinerate a used film. are doing. |