http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08236146-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_345d74727e77e6d36988fd1168fb2589 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0950e9df7f0e1b73efee1bda859951ad |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-30 |
filingDate | 1995-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_079641c49a0236c484db30f756937e92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a833d2c71de2fb43b95078875da48e4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fc459181166a29eee8c6c2204d4dfbb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d0173577441598a2782ebdedbf8daf6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6071a0a96ffe0c3cef97515a656c2a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_39b7cb243c920c091405156c5c3bb89b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1785f5f0d0e680d66230499a9c4bfdce http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f46a508318e28b50e1ef0afc659cbbe |
publicationDate | 1996-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08236146-A |
titleOfInvention | Method for manufacturing nickel-metal hydride storage battery |
abstract | (57) [Summary] [Objective] To provide a manufacturing method of a nickel-hydrogen storage battery capable of suppressing the capacity reduction after being left for a long time and effectively utilizing the thermal energy used in the initial charging step. It is what A step of producing an electrode group by interposing and insulating a non-sintered nickel positive electrode containing nickel oxide and cobalt oxide and a negative electrode containing a hydrogen-absorbing alloy with a separator made of a polymer nonwoven fabric interposed therebetween, Storing the electrode group in an airtight container together with an alkaline electrolyte, 40-1 A step of performing an initial charge at a high temperature of 20 ° C., and a sealed container after the initial charge by exchanging heat between the sealed container after the initial charge and the sealed container that stores the electrode group and the alkaline electrolyte that have not been charged yet. And heating the non-initially charged closed container. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016197588-A |
priorityDate | 1995-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 47.