http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08231635-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6cfc033f059d282fcd915bc8be2ae53f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-06 |
filingDate | 1995-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c0aa93738cad7758463676a8835aff28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17e697acb38713a8e1f1dd8a79863099 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1d331266a5fa47c4d5e00dd459812e91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0f8a059a35b14eadf39ccfeb7e75e67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_588671a45f55a131360877f9a0e53353 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8ab64ae83bdca62078cce3fcd2dbf12 |
publicationDate | 1996-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08231635-A |
titleOfInvention | Continuous production method of ABS resin having improved gloss |
abstract | (57) [Summary] [Structure] A raw material containing a styrene-based monomer, an acrylonitrile-based monomer, and a rubber-like polymer is supplied to a polymerization step to produce a rubber-like polymer particle (rubber particle). After polymerization of the monomer, the monomer and / or solvent is introduced into a decompression chamber to separate the monomer component and / or the solvent from the resin component, and then is introduced into an extruder after the collecting step, and the product is passed through the extruder. In the continuous method for producing an ABS resin by a solution or bulk polymerization method, a part to which water is added, a part to evaporate water to the outside, a resin in the extruder are added between the recovery process outlet and the extrusion process outlet. A method for producing an ABS resin, which comprises two or more sets of combinations of X, Y, and Z parts consisting of screw element parts for kneading, and adding and removing a specific amount of water. [Effect] It is possible to easily manufacture a resin having a dramatically improved balance of physical properties such as impact strength and surface gloss after molding. |
priorityDate | 1995-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |