http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08217802-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-06 |
filingDate | 1995-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_74494ac069d1bb4935d1894bf7d22771 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_812288359f38d52befcb14300083368f |
publicationDate | 1996-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08217802-A |
titleOfInvention | Process for producing polymer having reduced low-polymerization products and unreacted products |
abstract | (57) [Summary] [Object] The present invention provides a method for producing a water-soluble polymer which is excellent in tackiness, thickening property and cohesiveness and in which a small amount of unpolymerized substances and unreacted substances are small. [Structure] In producing a water-soluble polymer having a low molecular weight of 10,000 or less and reduced unreacted materials, (1) When the polymerization rate reaches 90%, the viscosity of the polymerization system becomes 1 A step of carrying out an aqueous solution polymerization so as to be at least 0,000 cps, A water-soluble polymer comprising a step of (2) continuously polymerizing until the polymerization rate exceeds 95%, and a step of (3) ultrafiltering the obtained water-soluble polymer. Production method. |
priorityDate | 1995-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |