Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_eece3f4c4266dfce4fc469ddcb3eb4e9 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D30-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C5-14 |
filingDate |
1995-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_961a5a77887e9be46afac2a61807f742 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_209d1105cd926bfea7544a968557d64c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d7c6f5911de066517a867c5757fc82b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b766aca38b2eea58ce402a8120340b79 |
publicationDate |
1996-08-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H08216285-A |
titleOfInvention |
Pneumatic tire and manufacturing method thereof |
abstract |
(57) [Abstract] [Purpose] It is possible to reduce the weight of a tire by using an air permeation preventive layer that has excellent adhesion to the rubber layer and excellent water resistance and heat resistance, without impairing the air pressure retention inside the tire. And a method for manufacturing the same. [Structure] (1) (i) Polycopolymerized polyamide-based resin, (Ii) A pneumatic tire having an air permeation preventive layer formed of a thin film obtained by curing a liquid composition containing a curing resin and (iii) a curing agent that cures the curing resin, and the liquid composition before vulcanization Surface of the carcass layer of the green tire or the tire after vulcanization (or the surface of the rubber layer provided on the surface) The method for producing a pneumatic tire in which the air permeation preventive layer is formed by applying the composition after the halogenation treatment and / or after applying the adhesive and curing the composition. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9546266-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012007092-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104085257-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8933172-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104085257-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011161981-A1 |
priorityDate |
1995-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |