http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08209451-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-84 |
filingDate | 1995-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_619ce6fc37481fbb18594f4cad598ee6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0ce2b96156c11cbeb709ef5a68f0d42a |
publicationDate | 1996-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08209451-A |
titleOfInvention | Polyester composite fiber |
abstract | (57) [Summary] [Purpose] Stretchability, satisfying both processability, elimination of deterioration of productivity and crimp development after crimp development treatment, Provided is a polyester composite fiber having a latent crimping performance capable of obtaining a fabric and a non-woven fabric having an excellent elastic recovery property. [Structure] A polyethylene terephthalate-based polyester or a polybutylene terephthalate-based polyester copolymerized with a compound having a norbornane skeleton, and the polyester are eccentrically joined, and the number of latent crimps at 130 ° C. Is 40 fibers / 25 mm or more, and the number of crimps before crimping is 13 fibers / 25 mm or less. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-100419144-C http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-03046266-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6309719-B1 |
priorityDate | 1995-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |