http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08208846-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b0977255f940397ca6bbbb3f5cd7e1db |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 |
filingDate | 1995-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d7e31671e9b523358652c4f1e779297b |
publicationDate | 1996-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08208846-A |
titleOfInvention | Method for producing dry porous cellulose particles |
abstract | (57) [Summary] [Purpose] To produce dry porous cellulose particles having high strength, high porosity, and liquid absorbency associated with the porosity. [Structure] After freezing the porous cellulose particles swollen with water, and drying the frozen particles with hot air, dry porous cellulose particles having high strength and rich liquid absorbing property due to porosity are obtained. can get. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5988121-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7763348-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9830620-A1 |
priorityDate | 1995-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 18.