Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7ad58d3c0b071069a8ee0cb8c8ba2e8 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08C19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F36-04 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-60 |
filingDate |
1995-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6bfa5719d7b29ee6376d1e7d3e9e8d0b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9baba58d83013709cedff4cd685336af http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03ca4d8cfe801364b962c0f4b5fbbae3 |
publicationDate |
1996-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H08208751-A |
titleOfInvention |
Process for producing diene rubbers polymerized with Nd catalysts and exhibiting reduced cold flow and low inherent odor |
abstract |
Kind Code: A1 Abstract: A method for producing a diene rubber having good rubber technical characteristics and reduced cold flow by the energetically desirable route and without unpleasant inherent odor. The preparation of diene rubbers polymerized by Nd catalysts and having reduced cold flow and low inherent odors is carried out in the presence of an inert organic solvent and in the presence of a neodymium carboxylate-based metal-organic mixed catalyst. So- By adiabatically polymerizing the diolefins at a temperature of 20 ° C. to 150 ° C., subsequently depressurizing the reaction mixture obtained in this way by reducing the pressure, and thereafter diluting the reaction mixture with disulphur dichloride. , Sulfur dichloride and / or thionyl chloride. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015040295-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016534170-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015513587-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018197354-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20160079811-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9822195-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016535130-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6664347-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20210079425-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11713365-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2022510646-A |
priorityDate |
1994-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |