http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08208722-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d9cb217f83556ce2a418344c2d485415 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 |
filingDate | 1995-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e686ff3a2ff12b9019199370421f6f0c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31ba0a1c93ef177afdbaf2861df2e441 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8bda0a5e1f959655511381fe348c6fab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8fb0f35aad44e5167ecb7ef52d104df3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac97bce3576e3b726ccba9e9cd7051db |
publicationDate | 1996-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08208722-A |
titleOfInvention | Method for producing polybutadiene |
abstract | (57) [Summary] [Structure] (A) An aging liquid obtained by contacting a transition metal compound with a Group I to III organometallic compound in the presence of a conjugated diene to be polymerized, and (B) carbon disulfide, Using a catalyst obtained from a compound selected from the group consisting of phenyl isothiocyanate and a xanthate compound, (C) a specific gravity of 1.1 (20 ° C.) in the presence of an inert organic solvent having a high specific gravity of 20 ° C. or more, a method of batch-wise polymerizing a monomer having a conjugated diene as a main component to be polymerized in a water-based polymerization medium, (1) A part of the (A), (B) and (C) is added to the polymerization medium to start the polymerization, and (2) the rest of the (A), (B) and (C) is continuously added. Or a method of producing polybutadiene, characterized in that the polybutadiene is maintained at a predetermined polymerization temperature by intermittently or intermittently. [Effect] A runaway reaction can be prevented and stable polymerization can be performed. Since the heat of polymerization is used to raise the temperature, a heating device for the polymerization tank is unnecessary. Also, the molecular weight of SPB can be controlled. |