http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08203784-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-004 |
filingDate | 1995-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de331036700da249c2c87e20ec00d205 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d2c8e1b7e73fc7ea3a2955bc1aa35859 |
publicationDate | 1996-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08203784-A |
titleOfInvention | Solid electrolytic capacitor |
abstract | (57) [Abstract] [Purpose] To provide a solid electrolytic capacitor having excellent moisture resistance load characteristics. [Structure] A dielectric oxide film layer is formed on the surface of an anode substrate made of a valve action metal foil which is etched to a depth of 30 μm or more, Semiconductor layers composed of lead dioxide and lead sulfate are sequentially formed, The semiconductor layer has a capacitance equivalent to 8 in the etching pores. Solid electrolytic capacitor impregnated with 5% or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109791843-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109791843-A |
priorityDate | 1995-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 23.