http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08156121-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2f8cfa5aee4410611b5c562275c9f8e3 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29D7-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 1994-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0706eee4d109077b6b79a4afcc4058e1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e138da708cb682b612900bb791f4de03 |
publicationDate | 1996-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08156121-A |
titleOfInvention | Easy tear film and method for producing the same |
abstract | (57) [Summary] [Purpose] Tearability of films containing incompatible resins, Increases transparency and foldability. [Structure] Polyalkylene terephthalate (A) such as polybutylene terephthalate, styrene polymer (B) such as polystyrene and the following formula (I): A resin composition containing a polyether (C) containing a repeating unit represented by is extruded to obtain an easily tearable film. X is a divalent group obtained by removing hydrogen atoms from two hydroxyl groups of bisphenol A, Y is a 2-hydroxytrimethylene group, n is a natural number, and p is 10 to 10. An integer of about 1000 is shown. The ratio of the component (A) and the component (B) is the former (A) / the latter (B) = 45 / 55-90. / 10 (weight ratio), the ratio of the component (C) is 0.1 with respect to 100 parts by weight of the total amount of the components (A) and (B). It is about 30 parts by weight. |
priorityDate | 1994-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |