http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08127179-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-26 |
filingDate | 1994-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1578c32a2d30d1be089c3661c777d8aa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_84eed62d6e7c4205cffe76532af303a7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_959a047849378e7f63cf13b198ada04f |
publicationDate | 1996-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08127179-A |
titleOfInvention | Thermal recording material |
abstract | (57) [Summary] [Purpose] To obtain a heat-sensitive recording material having excellent water resistance and excellent disaggregation property during recycling of used paper. A thermosensitive recording material comprising a support and a thermosensitive coloring layer containing a leuco dye and a color developer as main components, wherein the support is JIS after being immersed in water at 20 ° C. for 30 minutes. Measure the tear strength values specified in P8116 according to JIS The value divided by the measured value of the basis weight specified in P8124 is 0. 3 or less paper is used, and the formed thermal recording material is 2 JIS P8116 after immersion in water at 0 ° C for 30 minutes A heat-sensitive recording material having a measured tear strength of 30 g or more. |
priorityDate | 1994-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |