http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08123098-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-113 |
filingDate | 1994-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_710f8df59599976a23b61cff7aec0da1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8d5c96fae222513d954aafb8680b6e18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_057e55e8ebd0a8fd4816620ab112bfc4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_731aaeb876baab580d4e0c1a15ad31f4 |
publicationDate | 1996-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08123098-A |
titleOfInvention | Two-component developer |
abstract | (57) [Summary] [Structure] A two-component developer comprising a toner and a coated carrier for developing an electrostatic latent image, wherein a polytitanocarbosilane polymer is used as a coating material. Component developer. [Effect] The two-component developer of the present invention does not peel or damage the carrier core material and the coating layer even after long-term use, and prevents the spent of the toner. Therefore, the charge amount is reduced and the toner is scattered. Therefore, the inside of the copying machine is not contaminated and the image quality is not deteriorated. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010224054-A |
priorityDate | 1994-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 78.