http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H08120030-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6cfc033f059d282fcd915bc8be2ae53f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-00 |
filingDate | 1994-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c0aa93738cad7758463676a8835aff28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8ab64ae83bdca62078cce3fcd2dbf12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17e697acb38713a8e1f1dd8a79863099 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f0f8a059a35b14eadf39ccfeb7e75e67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1d331266a5fa47c4d5e00dd459812e91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_588671a45f55a131360877f9a0e53353 |
publicationDate | 1996-05-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H08120030-A |
titleOfInvention | Continuous production method of ABS resin having good physical property balance |
abstract | (57) [Summary] [Structure] A solution which is obtained by passing through a polymerization step for polymerizing ABS, and then through a separation and recovery step, introducing into the extruder after the recovery step, and passing through the extruder to obtain a product. Alternatively, in the continuous production method of the ABS resin by the bulk polymerization method, water is added to the resin in the step, and at the same time and / or after addition, the resin is allowed to pass through a high shear region, and the added water represented by the following formula is evaporated. The heat H lost from the resin is 10 to 300 And a method for producing an ABS resin. H = Q / W Q: The amount of heat deprived from the resin per hour (kcal) W: The amount of extruded resin per hour (kg) [Effect] The balance of physical properties such as impact strength and surface gloss after molding is dramatically improved. The improved resin can be easily manufactured. |
priorityDate | 1994-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 61.