abstract |
(57) [Summary] [Purpose] To develop a rubber-modified styrene resin composition that maintains high rigidity, is excellent in impact resistance and gloss, and is excellent in fluidity. [Constitution] (A) Weight average molecular weight (Mw) is 100,000 In the continuous phase of 0 to 160,000 styrenic resin, (B) A rubber-modified styrene-based resin composition in which rubber-like polymer particles having specific properties having occluded particles in which a styrene-based resin is incorporated are dispersed. |