http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0782040-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_294881271413951a95f284b588a68e66 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-133 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01F41-02 |
filingDate | 1993-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a35233ed9248cbd14d66afe594d11563 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c30e5b55aa85c64af4f90c451666ae09 |
publicationDate | 1995-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0782040-A |
titleOfInvention | Ferrite core manufacturing method |
abstract | (57) [Summary] [Construction] A green sheet 7 is produced from the raw material slurry 3 by a doctor blade device 11, punched into a desired shape using a punch die, degreased, fired, and the like, and then a ferrite core, for example, A core for a magnetic modulation recording head and a core for a rotary transformer are manufactured. [Effect] Grinding is not necessary after firing and mass productivity is improved, so that manufacturing cost can be reduced. Further, it is possible to reuse the material of the unnecessary portion. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015081226-A |
priorityDate | 1993-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 23.