http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0781983-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B17-10 |
filingDate | 1993-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_baf7ffadd02c2ecc2f84bade6bd97618 |
publicationDate | 1995-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0781983-A |
titleOfInvention | Intermediate film for laminated glass |
abstract | (57) [Summary] [Object] To provide a resin-based interlayer film for laminated glass, which has excellent sound insulation properties and does not require addition of a plasticizer. [Structure] The main raw material of the interlayer film for laminated glass is an amorphous polyester resin composed of a polyvalent carboxylic acid and an aliphatic dihydric alcohol. The amorphous polyester resin has a glass transition temperature of -20 ° C to + 40 ° C and a melting start temperature of 100 ° C or lower. In particular, 0.1 to 3 mol% of all constituent monomers of the amorphous polyester resin is an aromatic dihydric alcohol represented by the following formula [I] or an aromatic divalent carboxylic acid represented by the following formula [II]. At least one of. (In the formula, n is 3 or 4, R 1 and R 2 are each independently an alkylene group, and l and m are each independently 0 or an integer of 1 or more.) (In the formula, p represents 3 or 4.) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015000821-A |
priorityDate | 1993-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 142.