http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0781227-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c6bb14de7280e28bba4f50c3061b6c3e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-337 |
filingDate | 1993-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3879ca9d211e388e96f555aef67788e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e92946dea469fe6d072573b9b974c536 |
publicationDate | 1995-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0781227-A |
titleOfInvention | Thermal recording |
abstract | (57) [Summary] [Purpose] To obtain a heat-sensitive recording material having a high gloss and a high recording density and having a good stick. [Structure] A thermosensitive coloring layer on at least one surface of a support, A thermal recording medium having an intermediate layer and a gloss layer, wherein the gloss layer contains an ionizing radiation curable resin having a glass transition temperature of 250 ° C. or higher and silicone oil. [Effect] It is possible to obtain a heat-sensitive recording material having a high gloss and a high recording density and having a good stick. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100332041-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8461076-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2364859-A2 |
priorityDate | 1993-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 115.