http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0770991-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9cb815fb0ce55fb7e1dc62164b9692cb |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02A40-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W90-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H21-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H21-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B31-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D5-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F9-16 |
filingDate | 1993-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_777410bc1fb4f033f35898826d88192c |
publicationDate | 1995-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0770991-A |
titleOfInvention | Method for producing special bamboo activated carbon sheet, corrugated cardboard box manufactured using this special bamboo activated carbon sheet, and corrugated cardboard box using special bamboo activated carbon |
abstract | (57) [Summary] [Purpose] To provide a special bamboo activated carbon sheet and corrugated ball box suitable for transportation and storage of so-called fresh food such as vegetables and fruits and fresh flowers. [Structure] Bamboo powder obtained by crushing bamboo pieces is about 170 ℃ -300 ℃ After heating in the range of 1, the special bamboo activated carbon produced by injecting steam of about 100 ° C. to 150 ° C. is crushed into the paper pulp fiber at a predetermined ratio to manufacture the first special bamboo activated carbon sheet. The first special bamboo activated carbon sheet is used as an inner layer paper or / and a cover sheet or an intermediate layer paper of a corrugated ball box to form a corrugated ball box. In addition, a mixture of both the bamboo powder activated carbon produced by a separate method and the above special bamboo activated carbon was squeezed into the paper pulp fiber at a predetermined ratio to produce a second special bamboo activated carbon sheet. It is also possible to form a corrugated ball box by using the bamboo activated carbon sheet and the inner layer paper as described above. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107985799-A |