http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0762304-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 |
filingDate | 1993-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_760e7b4b374334011b3cd6d2f65698a8 |
publicationDate | 1995-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0762304-A |
titleOfInvention | Adhesive tape manufacturing method |
abstract | (57) [Abstract] [Purpose] To provide a method for producing a pressure-sensitive adhesive tape which has sufficient adhesive strength at room temperature and can be easily re-peeled by performing a heat treatment at about 100 ° C with good productivity. To aim. A method for producing a pressure-sensitive adhesive tape, which comprises applying an acrylic photopolymerizable composition to a synthetic resin film or a fiber cloth sheet having a heat shrinkage of 5 to 80% and then irradiating it with ultraviolet rays. The removable adhesive tape obtained by the production method of the present invention has a high initial adhesive strength at room temperature and By performing the heat treatment at 0 ° C., the adhesive force can be reduced until the peeling can be easily performed. Furthermore, when the pressure-sensitive adhesive tape is manufactured, it does not require heat to form the pressure-sensitive adhesive layer, so that the pressure-sensitive adhesive tape can be directly applied to the base material, and the highly removable pressure-sensitive adhesive tape can be manufactured. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6048431-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015151473-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2340772-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/GB-2340772-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7105226-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104449542-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002088320-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7544414-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002088321-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100655036-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/SG-82017-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1130070-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6398892-B1 |
priorityDate | 1993-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 78.