http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0762178-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-00 |
filingDate | 1993-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_57be4231057e0ae28ef76b62b7e84f98 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d954f0a0fadfa3725697a1534a328c21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_210c8f5e46bf087ec856bc6f49ebb3c4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_64afa937728dda6c2133de9ce860bf38 |
publicationDate | 1995-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0762178-A |
titleOfInvention | Method for producing aromatic vinyl resin composition |
abstract | (57) [Summary] [Structure] 100 parts by weight of an aromatic vinyl resin (A) having a weight average molecular weight of 300,000 to 700,000, for example, a weight average molecular weight of 3 100 parts by weight of 50,000 polystyrene and 3 to 30 parts by weight of the aromatic vinyl resin (B) having a weight average molecular weight of 85,000 or less, for example, 10 parts by weight of polystyrene having a weight average molecular weight of 70,000 are used in an extruder or the like. A method for producing an aromatic vinyl-based resin composition, which is uniformly mixed using a kneader. [Effect] An aromatic vinyl resin composition having excellent fluidity and having no deterioration in mechanical strength and heat resistance can be easily obtained without a large increase in cost. |
priorityDate | 1993-08-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 75.