Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_345d74727e77e6d36988fd1168fb2589 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 |
filingDate |
1993-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b5e5efce73cf2743fbfd75d71968a93d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f71cada5e6693ee1e3797cd5809bde4d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b23e751a0653566f6953b311e618fc36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_35df78e70dc365b9c8b5cd1bbe3f2943 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d454b4873f222ceb257ef5fa9923cecc |
publicationDate |
1995-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0757735-A |
titleOfInvention |
Treatment method of paste type electrode for alkaline secondary battery |
abstract |
(57) [Summary] [Structure] In a method for treating cobalt oxide powder used as an active material mixture for a paste type electrode for an alkaline secondary battery, the cobalt oxide powder is treated at a relative humidity of 85 to 95% and a temperature of 25 to 28%. The method for treating cobalt oxide powder, which comprises subjecting to humidification and heating in air at a temperature of ℃. [Effect] While the active material utilization rate of the paste electrode is improved, a stable active material utilization rate with less variation can be obtained. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002503873-A |
priorityDate |
1993-08-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |