http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H075698-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-32 |
filingDate | 1993-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51fdffd7e4751c609dd9c0d09d866a08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_01c62705007583e053726f96bacf7f4b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d71ec52186acb538d7e6632acf5d59d1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4fd8b8543172e89baa54897492530dab |
publicationDate | 1995-01-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H075698-A |
titleOfInvention | Solidified developer for non-silver salt light-sensitive material and method for producing the same |
abstract | (57) [Summary] [Purpose] The load (weight and volume) on transportation and logistics can be reduced, the waste of packaging materials can be reduced, and it is a solid state that is easy to handle and can be easily dissolved, and there is no problem such as precipitation. Provided are a developer for a non-silver salt light-sensitive material capable of stable development for a long period of time, and a method for producing the same. [Structure] A developer for a non-silver salt light-sensitive material comprising a granular solid containing 10% by weight or more of an alkali metal silicate, A solidified developer having a porosity of 50% or less, and the solidified developer characterized by being solidified by a pressure compression method using an alkali metal silicate granulated by a spray drying method. Method of manufacturing agent. |
priorityDate | 1993-06-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |