http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0752538-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-382 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-26 |
filingDate | 1993-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ae193c092ab900954fdc855f09b233d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d8555c5f850715e24b23587976508b83 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_696667ce3e99000c22c56a7065081245 |
publicationDate | 1995-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0752538-A |
titleOfInvention | Photothermal conversion type heat mode recording material |
abstract | (57) [Abstract] [Purpose] High-sensitivity, good printability on a recording medium with low smoothness, and a photothermal conversion heat mode that does not cause cracks in the photothermal conversion layer during handling or application of the ink layer. Provide recording material. [1] A photothermal conversion heat mode recording material comprising at least a cushion layer, a photothermal conversion layer, and an ink layer laminated in this order on a support, the photothermal conversion layer having a breaking elongation of 10% or more. Photothermal conversion type heat mode recording material that is softened so that |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6680089-B2 |
priorityDate | 1993-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 30.