Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6ec98db0102cc54087022bd58b0e6799 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ee1c19da359446fb5c4f0458a57b783d |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-055 |
filingDate |
1993-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77e4a870fe701c6acc8961f509a6d00f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fcb20afa2d137ce0be9d1177b6511e2d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f11492c0a81cac2b97f546fdb35ad190 |
publicationDate |
1995-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-H0737765-A |
titleOfInvention |
Electrolytic capacitor |
abstract |
(57) [Abstract] [Purpose] To provide an electrolytic capacitor capable of obtaining a good reproduced sound. [Constitution] Oxygen plasma treatment is applied to the aluminum foil. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8668060-B2 |
priorityDate |
1993-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |