http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-H0733520-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1476752f2420c8f8eb53464cf7fc922b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G25-00 |
filingDate | 1993-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b6a46f57d5a3d9bd2c8d41cdad15ba8e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_24aa5648b6cb6627609908da58b97692 |
publicationDate | 1995-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-H0733520-A |
titleOfInvention | Method for producing composite perovskite oxide powder |
abstract | (57) [Abstract] [Purpose] To manufacture piezoelectric oxide powder that is fine, has high surface activity and is easily sintered, at low cost. [Structure] General formula: (Pb 1-x M x ) (Ti 1-y Zr y ) O 3 (M is at least one rare earth element, 0 ≦ x ≦ 1, 0 ≦ y ≦ 1. ) To prepare an acidic mixed solution containing ions of each constituent element constituting the complex perovskite type oxide, hydrogen peroxide is added to the acidic mixed solution to obtain a precursor solution, The precursor is pyrolyzed. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8999573-B2 |
priorityDate | 1993-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 48.